Ni212 stranded wire Nickel Manganese Wire

Density
8.86 g/cm3 0.320 lb/in3
Melting point
1446oC 2635oF
Coefficient of expansion
12.9 µm/m °C (20 -100°C) 7.2 x 10-6 in/in °F(70 -212°F)
Modulus of rigidity
78 kN/mm2 11313 ksi
Modulus of elasticity
196 kN/mm2 28400 ksi