High temperature alloy A-286 Nimonic80A Nimonic90 Nimonic75 cobalt alloy L605 bar

Physical constants and thermal properties/      Typical mechanical properties (room temperature)
Density
9,27 g/cm³
Yield strength
min. 460 MPa
Melting point
1330 - 1410 °C
Tensile strength
min. 1000 MPa
Thermal conductivity
9,4 W/m · °C
Elongation
min. 50%
Coefficient of expansionat 21 - 93°C
13 μm/m · °C